Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 360 MPa @Temperature 100 °C |
52200 psi @Temperature 212 °F |
Wet; DIN65380 |
Hexcel® HexPly® M12 135°C Curing Epoxy Matrix, 37%/7781 Fiber Information provided by HexCel |