Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 3.00 - 172 MPa | 435 - 24900 psi | Average value: 51.2 MPa Grade Count:33 |
Overview of materials for Polyvinylidinefluoride (PVDF), Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polyvinylidinefluoride (PVDF), Molded/Extruded". Each property range of values reported is minimum and m.. |
|||
Compressive Yield Strength | 3.00 MPa | 435 psi | ASTM D395 |
Covestro Baydur® 646 Polyurethane Structural Foam RIM, Density 15 pcf, MDI-based 2-Component Liquid System 0.25 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and of.. |
|||
Compressive Yield Strength | >= 3.00 MPa | >= 435 psi | Bare, min |
Hexcel® HexWeb® CFC™-20-1/8-5.0 Composite Flooring Honeycomb Core Hexweb CFC™-20 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes and, after expanding to the hexagonal confiation, the block is dipp.. |