Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 34.0 - 207 MPa | 4930 - 30000 psi | Average value: 106 MPa Grade Count:6 |
Overview of materials for Polyamide-Imide, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polyamide-Imide, Molded". Each property range of values reported is minimum and maximum values of approp.. |
|||
Compressive Yield Strength | 34.0 - 97.0 MPa | 4930 - 14100 psi | Average value: 79.5 MPa Grade Count:4 |
Overview of materials for Nylon 66, Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum .. |
|||
Compressive Yield Strength | 34.0 MPa | 4930 psi | at 1% deformation; ASTM D695 |
Ascend Performance Materials VYDYNE® 21SP Nylon, General Purpose 1.4% Deformation under 14 MPa (2000 psi) load.Typical property data. VYDYNE is a registered trademark of Solutia Inc. |