Polymer Property : Compressive Yield Strength = 30000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 100 - 207 MPa
14500 - 30000 psi
Average value: 155 MPa Grade Count:4
Overview of materials for Polyphthalamide (PPA), 20% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are..
Compressive Yield Strength 34.0 - 207 MPa
4930 - 30000 psi
Average value: 106 MPa Grade Count:6
Overview of materials for Polyamide-Imide, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polyamide-Imide, Molded". Each property range of values reported is minimum and maximum values of approp..
Compressive Yield Strength 103 - 207 MPa
15000 - 30000 psi
Average value: 157 MPa Grade Count:13
Overview of materials for Nylon 66, 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Glass Fiber Filled". Specific grades with glass content between 15% and 24% are included. ..
Compressive Yield Strength 103 - 207 MPa
14900 - 30000 psi
Average value: 172 MPa Grade Count:3
Overview of materials for PEKK, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "PEKK, Unreinforced". Each property range of values reported is minimum and maximum values of appropriate..