Polymer Property : Compressive Yield Strength = 5.38 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength >= 5.38 MPa
>= 780 psi
Stabilized, min
Hexcel® HexWeb® CR III 1/16-5052-.0007 Corrosion Resistant Specification Grade Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR..
Compressive Yield Strength >= 5.38 MPa
>= 780 psi
Bare, min
Hexcel® HexWeb® HRH-10 - 3/16 - 6.0 Aramid Fiber/Phenolic Resin Honeycomb
Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h..
Compressive Yield Strength 5.38 MPa
780 psi
Stabilized, typ
Hexcel® HexWeb® HRH-327 - 3/16 - 6.0 Fiberglass Reinforced Polyimide Honeycomb
Designation: Material-Cell Size (inches)-DensityHexWeb® HRH-327 is a glass-fabric, bias weave reinforced plastic honeycomb that incorporates a polyimide resin system for the node adhesive as well a..
Compressive Yield Strength >= 5.38 MPa
>= 780 psi
Stabilized, min, preliminary value obtained from limited testing
Hexcel® HexWeb® CFC™-20-1/8-6.0 Composite Flooring Honeycomb Core
Hexweb CFC™-20 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes and, after expanding to the hexagonal confiation, the block is dipp..