Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | >= 5.38 MPa | >= 780 psi | Stabilized, min |
Hexcel® HexWeb® CR III 1/16-5052-.0007 Corrosion Resistant Specification Grade Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR.. |
|||
Compressive Yield Strength | >= 5.38 MPa | >= 780 psi | Bare, min |
Hexcel® HexWeb® HRH-10 - 3/16 - 6.0 Aramid Fiber/Phenolic Resin Honeycomb Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h.. |
|||
Compressive Yield Strength | 5.38 MPa | 780 psi | Stabilized, typ |
Hexcel® HexWeb® HRH-327 - 3/16 - 6.0 Fiberglass Reinforced Polyimide Honeycomb Designation: Material-Cell Size (inches)-DensityHexWeb® HRH-327 is a glass-fabric, bias weave reinforced plastic honeycomb that incorporates a polyimide resin system for the node adhesive as well a.. |
|||
Compressive Yield Strength | >= 5.38 MPa | >= 780 psi | Stabilized, min, preliminary value obtained from limited testing |
Hexcel® HexWeb® CFC™-20-1/8-6.0 Composite Flooring Honeycomb Core Hexweb CFC™-20 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes and, after expanding to the hexagonal confiation, the block is dipp.. |