Polymer Property : Compressive Yield Strength = 50800 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 6.89 - 350 MPa
1000 - 50800 psi
Average value: 161 MPa Grade Count:21
Overview of materials for Epoxy Molding Compound
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Molding Compound". Each property range of values reported is minimum and maximum values of appropr..