Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 51.7 - 131 MPa | 7500 - 19000 psi | Average value: 81.6 MPa Grade Count:8 |
Overview of materials for Liquid Crystal Polymer (LCP), Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), Mineral Filled". Each property range of values reported is minimum and max.. |
|||
Compressive Yield Strength | 51.7 MPa | 7500 psi | Average value: 51.7 MPa Grade Count:3 |
Overview of materials for Polypropylene with 40% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Talc Filler". Specific grades with primary filler content between 35% and 44% are.. |
|||
Compressive Yield Strength | 51.7 MPa | 7500 psi | TM R050-38 |
Resinlab® EP1190 Flame Retardant Epoxy Casting Resin Resinlab™ EP1190 is a medium viscosity, flame retardant epoxy casting resin system. It is recognized under the Component Recognition Program of Underwriters Laboratories Inc., (File# E186034, Proje.. |