Polymer Property : Compressive Yield Strength = 52100 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 164 - 359 MPa
23800 - 52100 psi
Average value: 258 MPa Grade Count:7
Overview of materials for Phenolic, Carbon Fiber Composite
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Carbon Fiber Composite". Each property range of values reported is minimum and maximum values ..