Polymer Property : Compressive Yield Strength = 64000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 441 MPa
64000 psi
ATI Allegheny Ludlum Stainless Steel Type 201, 10% Cold Work (UNS S20100)
Allegheny Ludlum Type 201 and 201L have the greatest tonnage of the Cr-Ni-Mn steels (200 series). Type 201 provides advantages over the 18-8 grades in certain applications. Lower cost manganese an..