Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 5.00 MPa | 725 psi | at 1% nominal strain; ISO 604 |
Quadrant EPP Cestlite™ ASTL Polyethylene Data provided by Quadrant Engineering Plastic Products for polymers in their European product line. |
|||
Compressive Yield Strength | 5.00 - 15.2 MPa | 725 - 2200 psi | Average value: 7.11 MPa Grade Count:6 |
Overview of materials for Polyperfluoroalkoxyethylene (PFA), Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polyperfluoroalkoxyethylene, Molded/Extruded". Each property range of values reported is minimum and max.. |
|||
Compressive Yield Strength | 5.00 - 15.2 MPa | 725 - 2200 psi | Average value: 6.57 MPa Grade Count:9 |
Overview of materials for Fluorinated Ethylene Propylene (FEP), Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Fluorinated Ethylene Propylene (FEP), Molded/Extruded". Each property range of values reported is minimu.. |
|||
Compressive Yield Strength | 5.00 - 6.00 MPa @Strain 1.00 % |
725 - 870 psi @Strain 1.00 % |
ASTM D695 |
Guarniflon PTFE G800 Polytetrafluoroethylene A virgin PTFE with low coefficient of friction, excellent chemical inertness, non-adhesive surface, wide service temperature range, and excellent dielectric propertiesInformation provided by Guarnif.. |
|||
Compressive Yield Strength | >= 5.00 MPa | >= 725 psi | Bare, min, preliminary value obtained from limited testing |
Hexcel® HexWeb® CFC™-20-1/8-6.0 Composite Flooring Honeycomb Core Hexweb CFC™-20 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes and, after expanding to the hexagonal confiation, the block is dipp.. |