Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Modulus 0.0300 GPa
4.35 ksi
average; perpendicular to plane; DIN 53421
3A Composites Core Materials AIREX® R63.50 Damage Tolerant Foam
AIREX® R63 is a closed-cell, linear, thermoplastic polymer foam with high damage tolerance. This one of a kind formula combines very high elongation and excellent bond strength. AIREX® R63 is cold..
Compressive Modulus 0.0300 GPa
4.35 ksi
Elasticity; Short term E; DIN EN 826
BASF Styrodur® 4000 CS Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..