Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

3A Composites Core Materials AIREX® R63.50 Damage Tolerant Foam

Category Other Engineering Material , Composite Core Material , Polymer , Thermoplastic
Manufacturer 3A Composites Core Materials
Trade Name AIREX®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3A Composites Core Materials AIREX® R63.50 Damage Tolerant Foam.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
AIREX® R63 is a closed-cell, linear, thermoplastic polymer foam with high damage tolerance. This one of a kind formula combines very high elongation and excellent bond strength. AIREX® R63 is cold formable to simple shapes and thermo-formable to complex three-dimensional curves, and is nonfriable. AIREX® R63 is a core material for dynamically loaded and shock absorbing sandwich structures.CharacteristicsGood impact strength (non-brittle failure mode)Easy to thermoform (cold and hot)Dimensionally stableExcellent fatigue resistanceOutstanding core-to-skin adhesionNon biodegradableGood sound and thermal insulationApplicationsMarine: Hull bottoms, hull sidesRoad and Rail: Front-ends, side skirts, crash beltsAircraft: Explosion proof cargo containersRecreation: Surf boards, canoes, kayaksIndustrial: Containers, shelters, helmets
Physical Properties Metric English Comments
Density 0.0600 g/cc
0.00217 lb/in³
average; ISO 845
Mechanical Properties Metric English Comments
Tensile Strength 0.900 MPa
131 psi
average; in the plane; ISO 527 1-2
Elongation at Break 70 %
70 %
average; shear; ISO 1922
Tensile Modulus 0.0300 GPa
4.35 ksi
average; in the plane; ISO 527 1-2
Compressive Strength 0.380 MPa
55.1 psi
average; perpendicular to plane; ISO 844
Compressive Modulus 0.0300 GPa
4.35 ksi
average; perpendicular to plane; DIN 53421
Shear Modulus 0.0110 GPa
1.60 ksi
average; ASTM C393
Shear Strength 0.500 MPa
72.5 psi
average; ISO 1922
Charpy Impact, Notched 0.400 J/cm²
1.90 ft-lb/in²
DIN 53453
Thermal Properties Metric English Comments
Thermal Conductivity 0.0340 W/m-K
0.236 BTU-in/hr-ft²-°F
ISO 8301
Descriptive Properties Value Comments
Color brownish yellow
Users viewing this material also viewed the following: