Mechanical Properties Metric English Comments
Compressive Modulus 0.420 GPa
60.9 ksi
ASTM D695
Manifattura Cattaneo PTFE Polytetrafluoroethylene
Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a.
Compressive Modulus 0.420 GPa
60.9 ksi
ASTM D695
Manifattura Cattaneo RULON® J Polytetrafluoroethylene
Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a.