Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 0.420 GPa | 60.9 ksi | ASTM D695 |
Manifattura Cattaneo PTFE Polytetrafluoroethylene Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |
|||
Compressive Modulus | 0.420 GPa | 60.9 ksi | ASTM D695 |
Manifattura Cattaneo RULON® J Polytetrafluoroethylene Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |