Polymer Property : Compressive Modulus = 1.21 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Modulus 1.21 GPa
175 ksi
ASTM D695
Quadrant EPP Proteus® PP Natural Co-Polymer Polypropylene (ASTM Product Data Sheet)
Compressive Modulus 1.21 - 2.76 GPa
175 - 400 ksi
Average value: 2.30 GPa Grade Count:6
Overview of materials for Acetal Copolymer, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Unreinforced". Each property range of values reported is minimum and maximum values of..
Compressive Modulus 1.21 GPa
175 ksi
ASTM D695
Quadrant EPP Semitron® ESd 225, Extruded, Static Dissipative Acetal (ASTM Product Data Sheet)