Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Quadrant EPP Proteus® PP Natural Co-Polymer Polypropylene (ASTM Product Data Sheet)

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Quadrant Engineering Plastics Products
Trade Name Proteus®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Quadrant EPP Proteus® PP Natural Co-Polymer Polypropylene (ASTM Product Data Sheet).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Specific Gravity 0.900 g/cc
0.900 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore D 72
72
ASTM D2240
Tensile Strength 23.4 MPa
3400 psi
ASTM D638
Elongation at Break 300 %
300 %
ASTM D638
Tensile Modulus 1.05 GPa
152 ksi
ASTM D638
Flexural Strength 33.1 MPa
4800 psi
ASTM D790
Flexural Modulus 1.24 GPa
180 ksi
ASTM D790
Compressive Strength 33.1 MPa
4800 psi
10% Def.; ASTM D695
Compressive Modulus 1.21 GPa
175 ksi
ASTM D695
Izod Impact, Notched 4.27 J/cm
8.00 ft-lb/in
ASTM D256 Type A
Thermal Properties Metric English Comments
Melting Point 152 °C
305 °F
Crystalline, Peak; ASTM D3418
Maximum Service Temperature, Air 82.2 °C
180 °F
Long Term
Deflection Temperature at 1.8 MPa (264 psi) 100 °C
212 °F
ASTM D648
Flammability, UL94 HB
HB
1/8 inch (Estimated Rating)
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
Surface Resistivity per Square >= 1.00e+15 ohm
>= 1.00e+15 ohm
ASTM D257
Compliance Properties Metric English Comments
3A-Dairy Yes
Yes
Canada AG No
No
FDA Yes
Yes
NSF No
No
USDA No
No
USP Class VI No
No
Chemical Resistance Properties Metric English Comments
Acids, Strong (pH 1-3) Acceptable
Acceptable
Acids, Weak Acceptable
Acceptable
Alcohols Acceptable
Acceptable
Alkalies, Strong (pH 11-14) Acceptable
Acceptable
Alkalies, Weak Acceptable
Acceptable
Chlorinated Solvents Unacceptable
Unacceptable
Conductive / Static Dissipative No
No
Continuous Sunlight Limited
Limited
Hot Water / Steam Limited
Limited
Hydrocarbons - Aliphatic Unacceptable
Unacceptable
Hydrocarbons - Aromatic Unacceptable
Unacceptable
Inorganic Salt Solutions Acceptable
Acceptable
Ketones, Esters Unacceptable
Unacceptable
Descriptive Properties Value Comments
Color Natural
Machinability 3
1-10, 1=Easier to Machine
Users viewing this material also viewed the following: