Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 0.0100 GPa | 1.45 ksi | Elasticity; Long term E50; DIN EN 826 |
BASF Styrodur® 4000 CS Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Compressive Modulus | 0.0100 GPa | 1.45 ksi | 10% Compression Modulus; ASTM D695 |
Toyobo Pelprene™ S-1001 Polyester TPE Key Feature: Pelprene S typePelprene™ can be processed into a wide variety of articles from ultra-small precision parts to sheets by injection, extrusion, and blow molding. The 'S' type is a block.. |
|||
Compressive Modulus | 0.0100 GPa | 1.45 ksi | Elasticity; Short term E; DIN EN 826 |
BASF Styrodur® 2500 C Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |