Polymer Property : Compressive Modulus = 1.80 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Modulus 1.80 GPa
261 ksi
Sample Type A, 1 mm/min; ISO 604:2002
Global EPP PA 6C IMPACT Cast Polyamide 6 + Plasticizer
Cast nylons are generally accepted as the primary engineering polymer, suitable for virtually any plain bearing application. By varying the conditions of polymerisation the mechanical properties of ..
Compressive Modulus 1.80 GPa
261 ksi
ASTM D695
Cast Nylons Nycast® 6MPB Plasticized Nylon 6
A plasticized Type 6 material, NYCAST® 6MPB is formulated for use as pile driver caps or cushion pads. Data provided by the manufacturer, Cast Nylons Limited.The data below are average values prese..
Compressive Modulus 1.80 GPa
261 ksi
ASTM D695
Cast Nylons Nycast® 6MPY Plasticized Nylon 6
A plasticized Type 6 material, NYCAST® 6MPY is formulated for use as pile driver caps or cushion pads. Data provided by the manufacturer, Cast Nylons Limited.The data below are average values prese..
Compressive Modulus 1.80 GPa
261 ksi
Henkel Hysol EA 9313 Paste Adhesive System
Very low viscosity adhesive yielding tough, flexible bonds. Injectable.