Material Notes:
A plasticized Type 6 material, NYCAST® 6MPY is formulated for use as pile driver caps or cushion pads. Data provided by the manufacturer, Cast Nylons Limited.The data below are average values presented for comparison purposes. Actual property values may differ.
Physical Properties Metric English Comments
Density 1.15 g/cc
0.0415 lb/in³
ASTM D792
Water Absorption 0.50 %
0.50 %
24 hrs; ASTM D570
Water Absorption at Saturation 5.5 %
5.5 %
ASTM D570
Mechanical Properties Metric English Comments
Hardness, Rockwell R 112
112
ASTM D785
Hardness, Shore D 77
77
ASTM D2240
Tensile Strength, Ultimate 70.0 MPa
10200 psi
ASTM D638
Elongation at Break 25 - 35 %
25 - 35 %
ASTM D638
Tensile Modulus 2.80 GPa
406 ksi
ASTM D638
Flexural Yield Strength 86.0 MPa
12500 psi
ASTM D790
Flexural Modulus 2.30 GPa
334 ksi
ASTM D790
Compressive Yield Strength 162 MPa
23500 psi
10% Offset; ASTM D695
Compressive Modulus 1.80 GPa
261 ksi
ASTM D695
Shear Strength 72.0 MPa
10400 psi
ASTM D732
Izod Impact, Notched 0.500 J/cm
0.937 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 81.0 µm/m-°C

@Temperature 20.0 °C
45.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Melting Point 226 - 238 °C
439 - 460 °F
ASTM D789
Maximum Service Temperature, Air 110 °C
230 °F
Continuous service
166 °C
331 °F
Intermittent service
Deflection Temperature at 0.46 MPa (66 psi) 204 - 221 °C
399 - 430 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 166 - 204 °C
331 - 399 °F
ASTM D648
Electrical Properties Metric English Comments
Dielectric Constant 3.7

@Frequency 60 Hz
3.7

@Frequency 60 Hz
3.7

@Frequency 1000 Hz
3.7

@Frequency 1000 Hz
3.7

@Frequency 100000 Hz
3.7

@Frequency 100000 Hz
ASTM D150
Dielectric Strength 22.0 kV/mm
559 kV/in
Short time; ASTM D149