Polymer Property : Compressive Modulus = 2130 ksi
Polymer Property :
Compressive Modulus =
2130 ksi
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Compressive Modulus
14.7
GPa
2130
ksi
Phenolic 27%, Graphite fabric 73%
Phenolic - "91LD". Graphite fabric - "WCB"