Polymer Property : Compressive Modulus = 2470 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Modulus 8.41 - 17.0 GPa
1220 - 2470 ksi
Average value: 11.9 GPa Grade Count:3
Overview of materials for Phenolic, Carbon Fiber Composite
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Carbon Fiber Composite". Each property range of values reported is minimum and maximum values ..