Polymer Property : Compressive Modulus = 342 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Modulus 2.36 GPa
342 ksi
ASTM D695
Quadrant EPP Techtron® HPV PPS (ASTM Product Data Sheet)
Compressive Modulus 2.36 GPa

@Temperature 23.0 °C
342 ksi

@Temperature 73.4 °F
EN ISO 604
Ensinger TECASINT 4011 Polyimide, Yellow (PI)
TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel..
Compressive Modulus 2.36 GPa

@Temperature 23.0 °C
342 ksi

@Temperature 73.4 °F
EN ISO 604
Ensinger TECASINT 4201 SD Polyimide, Black, Carbon Fiber (PI)
TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel..
Compressive Modulus 2.36 GPa
342 ksi
ASTM D695
Arlon CuClad 250 PTFE/Woven Fiberglass Laminate Microwave Printed Circuit Board Substrate
CuClad 250 uses a higher fiberglass/PTFE ratio to provide mechanical properties approaching those of conventional substrates. Better dimensional stability and lower thermal expansion in all directi..
Compressive Modulus 2.36 GPa
342 ksi
ASTM-D-695
BCC Products EB 6200 Epoxy Tooling Board
EB6200 is a “grain-free” elevated temperature epoxy modeling material known for its superior surface finish, dimensional stability and the ability to maintain tolerances even after being subjected..