Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 2.40 GPa | 348 ksi | Type B, 5mm/min; ISO 604:2002 |
Nylacast Impact Nylon 6, Impact Grade Nylacast Impact has been designed for applications that have a high impact resistance and noise reduction capabilities. It works more effectively in applications where there are high stress. It also.. |
|||
Compressive Modulus | 2.40 GPa | 348 ksi | Sample Type A, 1 mm/min; ISO 604:2002 |
Global EPP PA 6C OFN Cast Polyamide 6 + Blended Liquid Lubricant Cast nylons are generally accepted as the primary engineering polymer, suitable for virtually any plain bearing application. By varying the conditions of polymerisation the mechanical properties of .. |
|||
Compressive Modulus | 2.40 GPa | 348 ksi | ASTM D695 |
Saint-Gobain Meldin® 7211 CM Compression Molded Graphite and PTFE Filled Polyimide Melidin® 7211 CM is a compression molded polyimide that contains 15% graphite and 10% PTFE fillers. This grade has the lowest coefficient of friction of the Meldin® 7000 series polyimides.Spe.. |
|||
Compressive Modulus | 2.40 GPa | 348 ksi | ASTM D695 |
Cast Nylons Nycast® Nyloil®-MDX Lubricated Nylon, MoS2 Filled NYCAST® NYLOIL® was developed to extend the wear-resistant properties of unlubricated or dry lubricated materials such as MoS2 filled nylons. NYCAST® NYLOIL® will last 5 to 7 times longer than .. |