Nylacast Impact Nylon 6, Impact Grade

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Impact Grade
Manufacturer Nylacast
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nylacast Impact Nylon 6, Impact Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Nylacast Impact has been designed for applications that have a high impact resistance and noise reduction capabilities. It works more effectively in applications where there are high stress. It also has good mechanical, thermal and chemical resistance properties.Information provided by Nylacast Ltd.
Physical Properties Metric English Comments
Density 1.11 g/cc
0.0401 lb/in³
method A; ISO 1183:1987
Mechanical Properties Metric English Comments
Tensile Strength, Yield 60.0 - 70.0 MPa
8700 - 10200 psi
Type 1B, 50mm/min; ISO 527-1/2:1993
Elongation at Break <= 10 %
<= 10 %
Type 1B, 50mm/min; ISO 527-1/2:1993
Tensile Modulus 3.25 GPa
471 ksi
Type 1B, 50mm/min; ISO 527-1/2:1993
Flexural Strength 93.5 MPa
13600 psi
1.5mm/min; ISO 178:2001
Flexural Modulus 2.40 GPa
348 ksi
1.5mm/min; ISO 178:2001
Compressive Strength 120 MPa
17400 psi
Type B, 5mm/min; ISO 604:2002
Compressive Modulus 2.40 GPa
348 ksi
Type B, 5mm/min; ISO 604:2002
Izod Impact, Notched (ISO) 13.9 kJ/m²
6.61 ft-lb/in²
Type A; ISO 180:2000
Thermal Properties Metric English Comments
CTE, linear 50.0 - 80.0 µm/m-°C

@Temperature 23.0 - 55.0 °C
27.8 - 44.4 µin/in-°F

@Temperature 73.4 - 131 °F
ISO 11359-2:1999
Melting Point 219.47 °C
427.05 °F
Maximum Service Temperature, Air 150 °C
302 °F
Intermittent
100 °C

@Time 1.80e+7 sec
212 °F

@Time 5000 hour
Continuous
Minimum Service Temperature, Air -100 °C
-148 °F
Intermittent
-40.0 °C
-40.0 °F
Continuous
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+17 ohm-cm
1.00e+17 ohm-cm
IEC 60093:1980-01
Surface Resistance 1.00e+15 ohm
1.00e+15 ohm
IEC 60093:1980-01
Dielectric Constant 3.7

@Frequency 1.00e+6 Hz
3.7

@Frequency 1.00e+6 Hz
IEC 60250:1969-01
4.0

@Frequency 100 Hz
4.0

@Frequency 100 Hz
IEC 60250:1969-01
Dielectric Strength 25.0 kV/mm
635 kV/in
IEC 60243-1:1998-01
Comparative Tracking Index 600 V
600 V
IEC 60112:2003-01
Descriptive Properties Value Comments
Color Grey