Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 2.50 GPa | 363 ksi | Type B, 5mm/min; ISO 604:2002 |
Nylacast Oilon Cast Nylon 6, Lubricated (Lubricant Oil Filled) This exceptional oil-loaded nylon features a complex blended oil lubrication system, uniformly distributed throughout the product, that guarantees constant performance over the whole service life. E.. |
|||
Compressive Modulus | 2.50 GPa | 363 ksi | ISO 604 |
Polikim KESTOIL® Polyamide 6 + Lubricant Kestoil® is a self-lubricated, strong, wear resistant engineering plastic with a low coefficient of friction. Implicit in its nature, it has many properties that no other material has in combinatio.. |
|||
Compressive Modulus | 2.50 GPa | 363 ksi | ASTM D695 |
Saint-Gobain Meldin® 7003 CM Compression Molded MoS2 Filled Polyimide Melidin® 7003 CM is a compression molded polyimide that includes 15% molybdenum disulfide self-lubricating filler for wear applications that operate in a vacuum or in very dry conditions.Specific.. |
|||
Compressive Modulus | 2.50 GPa | 363 ksi | ASTM D695 |
Saint-Gobain Meldin® 7003 Isostatically Molded Bearing Grade MoS2 Filled Polyimide Melidin® 7003 is a thermosetting polyimide that includes 15% molybdenum disulfide self-lubricating filler for wear applications that operate in a vacuum or in very dry conditions. Meldin® 700.. |