Material Notes:
This exceptional oil-loaded nylon features a complex blended oil lubrication system, uniformly distributed throughout the product, that guarantees constant performance over the whole service life. Excellent sliding frictional properties, abrasion resistance and stick/slip performance make this product a first choice for unlubricated moving parts.Information provided by Nylacast Ltd.
Physical Properties Metric English Comments
Density 1.138 g/cc
0.04111 lb/in³
method A; ISO 1183:1987
Mechanical Properties Metric English Comments
Hardness, Shore D 82 - 84
82 - 84
ISO 868:2003
Tensile Strength, Yield 70.0 - 75.0 MPa
10200 - 10900 psi
Type 1B, 50mm/min; ISO 527-1/2:1993
Elongation at Break >= 30 %
>= 30 %
Type 1B, 50mm/min; ISO 527-1/2:1993
Tensile Modulus 3.60 GPa
522 ksi
Type 1B, 50mm/min; ISO 527-1/2:1993
Flexural Strength 100 MPa
14500 psi
1.5mm/min; ISO 178:2001
Flexural Modulus 3.50 GPa
508 ksi
1.5mm/min; ISO 178:2001
Compressive Strength 95.0 MPa
13800 psi
Type B, 5mm/min; ISO 604:2002
Compressive Modulus 2.50 GPa
363 ksi
Type B, 5mm/min; ISO 604:2002
Izod Impact, Notched (ISO) 6.00 kJ/m²
2.86 ft-lb/in²
Type A; ISO 180:2000
Coefficient of Friction, Dynamic 0.15

@Pressure 1.75 MPa
0.15

@Pressure 254 psi
31.4m/min
K (wear) Factor 120 x 10-8 mm³/N-M

@Pressure 1.75 MPa
59.6 x 10-10 in³-min/ft-lb-hr

@Pressure 254 psi
31.4m/min
Thermal Properties Metric English Comments
CTE, linear 80.0 µm/m-°C

@Temperature 23.0 - 55.0 °C
44.4 µin/in-°F

@Temperature 73.4 - 131 °F
ISO 11359-2:1999
Melting Point 221 °C
430 °F
Maximum Service Temperature, Air 170 °C
338 °F
Intermittent
110 °C

@Time 1.80e+7 sec
230 °F

@Time 5000 hour
Continuous
Minimum Service Temperature, Air -100 °C
-148 °F
Intermittent
-40.0 °C
-40.0 °F
Continuous
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
IEC 60093:1980-01
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
IEC 60093:1980-01
Dielectric Constant 3.7

@Frequency 1.00e+6 Hz
3.7

@Frequency 1.00e+6 Hz
IEC 60250:1969-01
4.0

@Frequency 100 Hz
4.0

@Frequency 100 Hz
IEC 60250:1969-01
Dielectric Strength 25.0 kV/mm
635 kV/in
IEC 60243-1:1998-01
Comparative Tracking Index 600 V
600 V
IEC 60112:2003-01
Descriptive Properties Value Comments
Color Green
Wear Rate 0.11 mg/km
31.4m/min, 1.75MPa