Mechanical Properties Metric English Comments
Compressive Modulus 2.76 GPa
400 ksi
Resinlab® EP1112 Clear Electronic Grade Epoxy Encapsulant
Resinlab™ EP 1112 Clear is a two part unfilled fast curing electronic grade epoxy encapsulant designed for small to medium sized castings. It cures completely at room temperature to a tough, flexib..
Compressive Modulus 2.76 GPa
400 ksi
ASTM D695
Quadrant EPP Acetron® POM-C Copolymer Acetal, Porosity-Free, Unfilled, Extruded
Compressive Modulus 2.76 GPa
400 ksi
ASTM D695
Quadrant EPP Ertalyte® TX Internally Lubricated Semi-Crystalline Polyester (ASTM Product Data Sheet)
Compressive Modulus 2.76 GPa
400 ksi
ASTM D695
Quadrant EPP Nylatron® GSM Nylon, Cast MoS2 Filled Type 6 (ASTM Product Data Sheet)
Compressive Modulus 2.76 GPa
400 ksi
ASTM D695
Quadrant EPP Nylatron® MC® 901 Blue, Heat Stabilized, Type 6 (ASTM Product Data Sheet)
Data provided by Quadrant Engineering Plastic ProductsBroadest size range availabilityGood mechanical and electrical propertiesIdeal balance of strength and toughnessCast as finished parts and near ..
Compressive Modulus 2.76 GPa
400 ksi
ASTM D695
Quadrant EPP Nylatron® NSM Nylon, Cast Solid Lubricant Filled, Type 6 (ASTM Product Data Sheet)
Compressive Modulus 2.76 GPa
400 ksi
ASTM D695
Quadrant EPP Nylatron® WP PA (ASTM Product Data Sheet)
Compressive Modulus 2.76 GPa
400 ksi
TM R050-38
Resinlab® EP1385 Black Epoxy Formulation
Resinlab™ EP1385 Black is an epoxy formulation designed for applications requiring resistance to E-85 type fuels. It has good wetting and adhesion to most surfaces. It has very good resistance to w..
Compressive Modulus 2.76 GPa
400 ksi
TM R050-38
Resinlab® EP1385 Clear Epoxy Formulation
Resinlab™ EP1385 Clear is an epoxy formulation designed for applications requiring resistance to E-85 type fuels. It has good wetting and adhesion to most surfaces. It has very good resistance to w..
Compressive Modulus 2.76 GPa
400 ksi
TM R050-38
Resinlab® EP1390 Medium Viscosity, Self Extinguishing Flame Retardant Epoxy Casting Resin System
Resinlab™ EP1390 is a RoHS compliant, medium viscosity, self extinguishing flame retardant epoxy casting resin system. It is recognized under the Component Recognition Program of Underwriters Labor..
Compressive Modulus 2.76 GPa
400 ksi
ASTM D695
Quadrant EPP Semitron® CMP LL5 Polyester (ASTM Product Data Sheet)
Enhanced semi-crystalline polyester product for extended service in CMP retaining rings. Superior performance, especially in oxide processes, and cost effective relative to standard ring materials. ..
Compressive Modulus 2.76 GPa
400 ksi
ASTM D695
Quadrant EPP Semitron® CMP XL20 (ASTM Product Data Sheet)
Compressive Modulus 2.76 GPa
400 ksi
ASTM D695
Quantum Acetal-Copolymer
Information provided by Quantum Advanced Engineering Plastics
Compressive Modulus 2.76 - 5.58 GPa
400 - 809 ksi
Average value: 4.34 GPa Grade Count:4
Overview of materials for Polyetherimide (PEI), 20% Glass Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, 20% Glass Fiber". Specific grades with glass content between 15% and 24% are included. E..
Compressive Modulus 2.76 GPa
400 ksi
ASTM D695
Spartech Polycast MP 1.25 (UL 752 Level 1) Cell Cast Acrylic
Description: Cell Cast AcrylicInformation provided by Spartech.
Compressive Modulus 2.76 GPa
400 ksi
ASTM D695
Spartech Polycast SAR HP 1.25 (UL 752 Level 3) Cell Cast Acrylic
Description: Cell Cast AcrylicInformation provided by Spartech.
Compressive Modulus 2.76 GPa
400 ksi
ASTM D695
Spartech Polycast SP 1.25 Cell Cast Acrylic
Description: Cell Cast AcrylicInformation provided by Spartech.
Compressive Modulus 2.76 GPa
400 ksi
Engineered Syntactic Systems AZ-40 Deep Water Syntactic Foam
Syntactic foams are a combination of hollow spheres, a resin matrix, and other additives. When combined and processed properly, the constituents form a lightweight homogeneous material having high c..
Compressive Modulus 2.76 GPa

@Temperature 22.8 °C
400 ksi

@Temperature 73.0 °F
ASTM D695
Quadrant EPP Duratron® U2100 OEI Extruded 10% Glass Reinforced Polyetherimide
Compressive Modulus 2.76 GPa
400 ksi
ASTM D695
Quadrant EPP Nylatron® MC® 907 Natural Nylon, Monocast® FDA Compliant, Unfilled Type 6 (ASTM Product Data Sheet)
Compressive Modulus 2.76 GPa
400 ksi
Resinlab® EP1112 Black Electronic Grade Epoxy Encapsulant
Resinlab™ EP 1112 Black is a two part unfilled fast curing electronic grade epoxy encapsulant designed for small to medium sized castings. It cures completely at room temperature to a tough, flexib..
Compressive Modulus 2.76 GPa
400 ksi
TM R050-38
Resinlab® EP1199 Black Unfilled Epoxy Adhesive
Resinlab™ EP1199 Black is a two part unfilled epoxy adhesive designed for bonding of metals, ceramics and most plastics. This product gives good resistance to water, salt spray, inorganic acids and..
Compressive Modulus 2.76 GPa
400 ksi
TM R050-38
Resinlab® EP11HT Gray Filled Epoxy Adhesive
Resinlab™ EP11HT Gray is a two part filled epoxy adhesive designed for bonding metals and plastics. It cures at room temperature to a tough, semi-rigid material. It has good wetting to most surfa..
Compressive Modulus 2.76 GPa
400 ksi
TM R050-38
Resinlab® EP1199 Clear Unfilled Epoxy Adhesive
Resinlab™ EP1199 Clear is a two part unfilled epoxy adhesive designed for bonding of metals, ceramics and most plastics. This product gives good resistance to water, salt spray, inorganic acids and..