Polymer Property : Compressive Modulus = 5.80 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Modulus 0.00500 - 0.0400 GPa
0.725 - 5.80 ksi
Average value: 0.0177 GPa Grade Count:6
Overview of materials for Expanded Polystyrene (EPS)
This property data is a summary of similar materials in the MatWeb database for the category "Expanded Polystyrene (EPS)". Each property range of values reported is minimum and maximum values of app..
Compressive Modulus 0.00500 - 0.0400 GPa
0.725 - 5.80 ksi
Average value: 0.0177 GPa Grade Count:6
Overview of materials for Polystyrene, Extrusion Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Extrusion Grade". Each property range of values reported is minimum and maximum values of a..