Polymer Property : Compressive Modulus = 0.725 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Modulus 0.00500 - 0.0400 GPa
0.725 - 5.80 ksi
Average value: 0.0177 GPa Grade Count:6
Overview of materials for Expanded Polystyrene (EPS)
This property data is a summary of similar materials in the MatWeb database for the category "Expanded Polystyrene (EPS)". Each property range of values reported is minimum and maximum values of app..
Compressive Modulus 0.00500 GPa
0.725 ksi
Elasticity; Long term E50; DIN EN 826
BASF Styrodur® 3035 CS Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Compressive Modulus 0.00500 - 0.0400 GPa
0.725 - 5.80 ksi
Average value: 0.0177 GPa Grade Count:6
Overview of materials for Polystyrene, Extrusion Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Extrusion Grade". Each property range of values reported is minimum and maximum values of a..
Compressive Modulus 0.00500 GPa

@Temperature 23.0 °C
0.725 ksi

@Temperature 73.4 °F
DIN 28090-2
Guarniflon SC 1600 Polytetrafluoroethylene Seal
SC series is a superior and unique material for gasket (flat Sealing) applications. The overall benefits of Guarniflon SC series over that of both conventional PTFE and competitive PTFE/filler blen..