Mechanical Properties Metric English Comments
Compressive Modulus 52.0 GPa

@Temperature 175 °C
7540 ksi

@Temperature 347 °F
After ageing at 70°C / 95% RH
Hexcel® HexPly® 922-1/35%/G926 180°C Curing Epoxy Matrix
5H satin/370g/m2 carbon fabric: FVC=60%Information provided by HexCel
Compressive Modulus 52.0 GPa

@Temperature 100 °C
7540 ksi

@Temperature 212 °F
Wet; DIN65380
Hexcel® HexPly® M12 135°C Curing Epoxy Matrix, 45% 46280 Fiber
Information provided by HexCel
Compressive Modulus 52.0 GPa

@Temperature 100 °C
7540 ksi

@Temperature 212 °F
Wet; DIN65380
Hexcel® HexPly® M12 135°C Curing Epoxy Matrix, TVR380/26% Fiber
Information provided by HexCel