Mechanical Properties Metric English Comments
Compressive Modulus 55.2 GPa
8000 ksi
ASTM D695
Greene Tweed Orthetek® WF Polyketone, Continuous Woven Carbon Fiber
Greene Tweed offers precision-molded thermoplastic components made from our high-performance Orthtek® composite materials for a variety of demanding medical and biotechnology applications. Ortht..
Compressive Modulus 55.2 GPa
8000 ksi
ASTM D695
Greene Tweed WRâ„¢ 575 PEEK, Bi-Directional Carbon Fiber Filled
WR®575 is a thermoplastic composite consisting of bi-directionally oriented carbon fibers in a PEEK matrix. The excellent wear resistance and the fiber orientation of WR575 makes this material i..