Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 0.0250 GPa @Temperature 200 °C |
3.63 ksi @Temperature 392 °F |
ISO 6721 |
BASF Ultrason S 6010 PSU Ultrason S 6010 is an unreinforced, high molecular weight injection-molding and extrusion grade with excellent chemical resistance (stress crack resistance) and good solubility in typical solvents (.. |