Polymer Property : Secant Modulus = 0.426 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus 0.426 GPa

@Strain 2.70 %,
Temperature 80.0 °C
61.8 ksi

@Strain 2.70 %,
Temperature 176 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® S600F40 NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)&l
Unreinforced Low Viscosity Polybutylene Terephthalate Crastin S600F40 NC010 is an unreinforced lubricated low viscosity polybutylene terephthalate resin for injection molding.Information provided by..
Secant Modulus 0.426 GPa

@Strain 23.0 %,
Temperature -40.0 °C
61.7 ksi

@Strain 23.0 %,
Temperature -40.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 100 BK602 Acetal (POM)  (Unverified Data**)
High Viscosity Acetal Homopolymer Delrin 100 is a high viscosity acetal homopolymer for use in easy to fill molds. Delrin 100 provides maximum toughness in the product line without modification and ..