Polymer Property : Secant Modulus = 1.51 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus 1.51 GPa

@Strain 5.60 %,
Temperature -20.0 °C
219 ksi

@Strain 5.60 %,
Temperature -4.00 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 900P NC010 Acetal (POM)  (Unverified Data**)
Low Viscosity Acetal Homopolymer with Improved Processing Delrin 900P is a low viscosity acetal homopolymer for injection molding. It has improved processing thermal stability good mechanical proper..
Secant Modulus 1.51 GPa

@Strain 5.60 %,
Temperature -20.0 °C
219 ksi

@Strain 5.60 %,
Temperature -4.00 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® FG900P NC010 Acetal (POM)  (Unverified Data**)
Low Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG900P is a low viscosity acetal homopolymer with improved thermal stability. It has been developed for consideration ..