Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 1.62 - 10.2 GPa @Temperature -40.0 - 100 °C |
235 - 1480 ksi @Temperature -40.0 - 212 °F |
Average value: 5.73 GPa Grade Count:1 |
Overview of materials for Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled". Specific grades with glass content between 15.. |
|||
Secant Modulus | 1.62 - 10.2 GPa @Strain 0.250 - 3.50 % |
235 - 1480 ksi @Strain 0.250 - 3.50 % |
Average value: 5.73 GPa Grade Count:1 |
Overview of materials for Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled". Specific grades with glass content between 15.. |
|||
Secant Modulus | 1.62 GPa @Strain 3.50 %, Temperature 100 °C |
235 ksi @Strain 3.50 %, Temperature 212 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK643FR NC010 Polybutylene Terephthalate (PBT) 20% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin SK643FR is a flame retardant 20% glass reinforced polybutylene terephthalate molding resin. It is recognized as UL94V-0 at 0.8.. |
|||
Secant Modulus | 1.62 GPa @Temperature 200 °C |
235 ksi @Temperature 392 °F |
ASTM D882 |
DuPont™ Kapton® 120FN616 Polyimide/FEP Composite Film 120 Gauge film structure consisting of a 25 µm (1 mil) base polyimide film with a 2.5 µm (0.1 mil) coating of Teflon® FEP on both sides.Kapton® Type HN film coated with Teflon® FEP fluoropolyme.. |
|||
Secant Modulus | 1.62 GPa @Strain 0.620 %, Temperature 23.0 °C |
235 ksi @Strain 0.620 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® ST820 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) Unreinforced Polybutylene Terephthalate with Excellent Impact Resistance Crastin ST820 NC010 is an unreinforced Super Tough polybutylene terephthalate resin for injection molding.Information provide.. |
|||
Secant Modulus | 1.62 GPa @Strain 6.00 %, Temperature -40.0 °C |
234 ksi @Strain 6.00 %, Temperature -40.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 500PE NC010 Acetal (POM)
(Unverified Data**) Medium Viscosity Acetal Homopolymer with Very Low Emissions Delrin 500PE NC010 (formerly DE20578) is a medium viscosity acetal homopolymer an enhanced version of Delrin 500P with very low VOC emissi.. |