Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 0.827 GPa @Strain 1.10 %, Temperature 100 °C |
120 ksi @Strain 1.10 %, Temperature 212 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 127UV NC010 Acetal (POM)
(Unverified Data**) UV Stabilized High Viscosity Acetal HomopolymerDelrin 127UV is a high viscosity acetal homopolymer with UV stabilizers developed for automotive interior applications. It has improvements in UV aging.. |
|||
Secant Modulus | 0.829 GPa @Strain 6.90 %, Temperature 0.000 °C |
120 ksi @Strain 6.90 %, Temperature 32.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 520MP NC010 Acetal (POM)
(Unverified Data**) 20% Teflon® Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Delrin 520MP is a medium viscosity acetal homopolymer containing 20% Teflon PTFE Micropowder. It is designe.. |
|||
Secant Modulus | 0.826 GPa @Strain 1.36 %, Temperature 40.0 °C |
120 ksi @Strain 1.36 %, Temperature 104 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® RS LC3090 NC010 Nylon 610
(Unverified Data**) Unreinforced Renewably Sourced High Viscosity Polyamide 610 Developed for Extrusion Zytel RS LC3090 NC010 is a renewable sourced polyamide 610 containing a miniumu of 60% renewably sourced ingredien.. |
|||
Secant Modulus | 0.828 GPa @Strain 10.0 %, Temperature 0.000 °C |
120 ksi @Strain 10.0 %, Temperature 32.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 500P NC010 Acetal (POM)
(Unverified Data**) Medium Viscosity Acetal Homopolymer with Improved Processing Delrin 500P is a medium viscosity acetal homopolymer for injection molding. It has improved processing thermal stability good mechanical .. |