Mechanical Properties Metric English Comments
Secant Modulus 9.4951 GPa

@Strain 1.02 %,
Temperature 0.000 °C
1377.2 ksi

@Strain 1.02 %,
Temperature 32.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Rynite® RE5329 BK503 Polyethylene Terephthalate (PET)  (Unverified Data**)
36% Glass Reinforced Polyethylene TerephthalateInformation provided by DuPont Performance Polymers