Polymer Property : Secant Modulus = 1380 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus 9.51 GPa

@Strain 0.350 %,
Temperature 0.000 °C
1380 ksi

@Strain 0.350 %,
Temperature 32.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® LW9330 NC010 PBT+SAN  (Unverified Data**)
30% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9330 NC010 is a 30% glass fiber reinforced polybutylene terephthalate blend for injection molding. I..
Secant Modulus 9.54 GPa

@Strain 1.4648 %,
Temperature -40.0 °C
1380 ksi

@Strain 1.4648 %,
Temperature -40.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® SK615SF NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)&l
30% Glass Reinforced Low Viscosity Polybutylene Terephthalate Developed for Super Fast Production Crastin SK615SF is a 30% glass fiber reinforced low viscosity polybutylene terephthalate for injecti..