Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 1.00 GPa @Strain 0.900 %, Temperature 100 °C |
145 ksi @Strain 0.900 %, Temperature 212 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 900P NC010 Acetal (POM)
(Unverified Data**) Low Viscosity Acetal Homopolymer with Improved Processing Delrin 900P is a low viscosity acetal homopolymer for injection molding. It has improved processing thermal stability good mechanical proper.. |
|||
Secant Modulus | 0.999 GPa @Strain 0.86806 %, Temperature 100 °C |
145 ksi @Strain 0.86806 %, Temperature 212 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® FG500P NC010 Acetal (POM)
(Unverified Data**) Medium Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG500P is a medium viscosity acetal homopolymer with improved thermal stability. It has been developed for consider.. |
|||
Secant Modulus | 1.00 GPa @Strain 0.900 %, Temperature 100 °C |
145 ksi @Strain 0.900 %, Temperature 212 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® FG900P NC010 Acetal (POM)
(Unverified Data**) Low Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG900P is a low viscosity acetal homopolymer with improved thermal stability. It has been developed for consideration .. |