Polymer Property : Secant Modulus = 1640 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus 11.3 GPa

@Strain 0.230 %,
Temperature 23.0 °C
1640 ksi

@Strain 0.230 %,
Temperature 73.4 °F
ISO 11403-1 -2
DuPont Performance Polymers Rynite® RE5329 BK503 Polyethylene Terephthalate (PET)  (Unverified Data**)
36% Glass Reinforced Polyethylene TerephthalateInformation provided by DuPont Performance Polymers