Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 11.4 GPa @Strain 0.265 %, Temperature 23.0 °C |
1650 ksi @Strain 0.265 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK645FR NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l 30% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin SK645FR is a flame retardant 30% glass reinforced polybutylene terephthalate molding resin. It is recognized as UL94V-0 at 0.7.. |
|||
Secant Modulus | 11.4 GPa @Strain 1.67 %, Temperature -20.0 °C |
1650 ksi @Strain 1.67 %, Temperature -4.00 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Rynite® 540SUV BK544 Polyethylene Terephthalate (PET)
(Unverified Data**) 40% Glass Reinforced UV Stabilized Polyethylene Terephthalate Developed for Extrusion and Injection Molding Rynite 540SUV BK544 is a 40% glass fiber reinforced UV stabilized modified polyethylene te.. |
|||
Secant Modulus | 11.4 GPa @Strain 1.85 %, Temperature -20.0 °C |
1650 ksi @Strain 1.85 %, Temperature -4.00 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Rynite® RE5264 NC010 Polyethylene Terephthalate (PET)
(Unverified Data**) 36% Glass Reinforced Polyethylene Terephthalate Rynite RE5264 NC010 is a 36% glass fiber reinforced color stabilized modified polyethylene terephthalate.Information provided by DuPont Performance Po.. |
|||
Secant Modulus | 11.4 GPa @Strain 1.41 %, Temperature 23.0 °C |
1650 ksi @Strain 1.41 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Rynite® RE5264 NC010 Polyethylene Terephthalate (PET)
(Unverified Data**) 36% Glass Reinforced Polyethylene Terephthalate Rynite RE5264 NC010 is a 36% glass fiber reinforced color stabilized modified polyethylene terephthalate.Information provided by DuPont Performance Po.. |
|||
Secant Modulus | 11.4 GPa @Strain 0.600 %, Temperature 23.0 °C |
1650 ksi @Strain 0.600 %, Temperature 73.4 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® PLS 95G40DH1T BK261 Nylon 6
(Unverified Data**) 40% Glass Reinforced Heat Stabilized Polyamide Zytel PLS95G40DH1T is a 40% GR impact modified PA made with SHIELD technology its superior heatInformation provided by DuPont Performance Polymers |