DuPont Performance Polymers Zytel® PLS 95G40DH1T BK261 Nylon 6  (Unverified Data**)

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 40% Glass Fiber Filled
Manufacturer DuPont Performance Polymers
Trade Name Zytel® PLS
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Zytel® PLS 95G40DH1T BK261 Nylon 6  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
40% Glass Reinforced Heat Stabilized Polyamide Zytel PLS95G40DH1T is a 40% GR impact modified PA made with SHIELD technology its superior heatInformation provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Density 1.43 g/cc
0.0517 lb/in³
DAM; ISO 1183
Linear Mold Shrinkage, Flow 0.0030 cm/cm
0.0030 in/in
DAM; ISO 294-4 2577
Linear Mold Shrinkage, Transverse 0.0080 cm/cm
0.0080 in/in
DAM; ISO 294-4 2577
Mechanical Properties Metric English Comments
Tensile Strength at Break 175 MPa
25400 psi
DAM; ISO 527-1/-2
Tensile Stress 17.41 MPa

@Strain 0.300 %,
Temperature 150 °C
2525 psi

@Strain 0.300 %,
Temperature 302 °F
DAM; ISO 11403-1 -2
25.48 MPa

@Strain 0.200 %,
Temperature 23.0 °C
3696 psi

@Strain 0.200 %,
Temperature 73.4 °F
DAM; ISO 11403-1 -2
26.55 MPa

@Strain 0.200 %,
Temperature -40.0 °C
3851 psi

@Strain 0.200 %,
Temperature -40.0 °F
DAM; ISO 11403-1 -2
33.05 MPa

@Strain 0.900 %,
Temperature 150 °C
4794 psi

@Strain 0.900 %,
Temperature 302 °F
DAM; ISO 11403-1 -2
42.1 MPa

@Strain 1.50 %,
Temperature 150 °C
6110 psi

@Strain 1.50 %,
Temperature 302 °F
DAM; ISO 11403-1 -2
49.83 MPa

@Strain 2.30 %,
Temperature 150 °C
7227 psi

@Strain 2.30 %,
Temperature 302 °F
DAM; ISO 11403-1 -2
77.78 MPa

@Strain 0.700 %,
Temperature 23.0 °C
11280 psi

@Strain 0.700 %,
Temperature 73.4 °F
DAM; ISO 11403-1 -2
84.47 MPa

@Strain 0.700 %,
Temperature -40.0 °C
12250 psi

@Strain 0.700 %,
Temperature -40.0 °F
DAM; ISO 11403-1 -2
111.24 MPa

@Strain 1.10 %,
Temperature 23.0 °C
16134 psi

@Strain 1.10 %,
Temperature 73.4 °F
DAM; ISO 11403-1 -2
133.7 MPa

@Strain 1.20 %,
Temperature -40.0 °C
19390 psi

@Strain 1.20 %,
Temperature -40.0 °F
DAM; ISO 11403-1 -2
145.83 MPa

@Strain 1.70 %,
Temperature 23.0 °C
21151 psi

@Strain 1.70 %,
Temperature 73.4 °F
DAM; ISO 11403-1 -2
180.23 MPa

@Strain 1.80 %,
Temperature -40.0 °C
26140 psi

@Strain 1.80 %,
Temperature -40.0 °F
DAM; ISO 11403-1 -2
Elongation at Break 4.0 %
4.0 %
DAM; ISO 527-1/-2
Tensile Modulus 11.3 GPa
1640 ksi
DAM; ISO 527-1/-2
Flexural Strength 277 MPa
40200 psi
DAM; ISO 178
Flexural Modulus 10.0 GPa
1450 ksi
DAM; ISO 178
Secant Modulus 1.77 GPa

@Strain 4.80 %,
Temperature 100 °C
257 ksi

@Strain 4.80 %,
Temperature 212 °F
DAM; ISO 11403-1 -2
2.41 GPa

@Strain 3.10 %,
Temperature 100 °C
350 ksi

@Strain 3.10 %,
Temperature 212 °F
DAM; ISO 11403-1 -2
3.78 GPa

@Strain 1.40 %,
Temperature 100 °C
549 ksi

@Strain 1.40 %,
Temperature 212 °F
DAM; ISO 11403-1 -2
5.19 GPa

@Strain 0.700 %,
Temperature 100 °C
753 ksi

@Strain 0.700 %,
Temperature 212 °F
DAM; ISO 11403-1 -2
6.36 GPa

@Strain 2.70 %,
Temperature 23.0 °C
923 ksi

@Strain 2.70 %,
Temperature 73.4 °F
DAM; ISO 11403-1 -2
8.09 GPa

@Strain 1.90 %,
Temperature 23.0 °C
1170 ksi

@Strain 1.90 %,
Temperature 73.4 °F
DAM; ISO 11403-1 -2
8.2575 GPa

@Strain 2.80 %,
Temperature -40.0 °C
1197.7 ksi

@Strain 2.80 %,
Temperature -40.0 °F
DAM; ISO 11403-1 -2
9.37 GPa

@Strain 0.100 %,
Temperature 100 °C
1360 ksi

@Strain 0.100 %,
Temperature 212 °F
DAM; ISO 11403-1 -2
9.6465 GPa

@Strain 2.00 %,
Temperature -40.0 °C
1399.1 ksi

@Strain 2.00 %,
Temperature -40.0 °F
DAM; ISO 11403-1 -2
10.1 GPa

@Strain 1.10 %,
Temperature 23.0 °C
1470 ksi

@Strain 1.10 %,
Temperature 73.4 °F
DAM; ISO 11403-1 -2
11.1 GPa

@Strain 1.20 %,
Temperature -40.0 °C
1620 ksi

@Strain 1.20 %,
Temperature -40.0 °F
DAM; ISO 11403-1 -2
11.4 GPa

@Strain 0.600 %,
Temperature 23.0 °C
1650 ksi

@Strain 0.600 %,
Temperature 73.4 °F
DAM; ISO 11403-1 -2
12.27 GPa

@Strain 0.600 %,
Temperature -40.0 °C
1780 ksi

@Strain 0.600 %,
Temperature -40.0 °F
DAM; ISO 11403-1 -2
13.38 GPa

@Strain 0.100 %,
Temperature 23.0 °C
1941 ksi

@Strain 0.100 %,
Temperature 73.4 °F
DAM; ISO 11403-1 -2
13.68 GPa

@Strain 0.100 %,
Temperature -40.0 °C
1984 ksi

@Strain 0.100 %,
Temperature -40.0 °F
DAM; ISO 11403-1 -2
Charpy Impact Unnotched 10.5 J/cm²
50.0 ft-lb/in²
DAM; ISO 179/1eU
Charpy Impact, Notched 2.10 J/cm²
9.99 ft-lb/in²
DAM; ISO 179/1eA
1.60 J/cm²

@Temperature -40.0 °C
7.61 ft-lb/in²

@Temperature -40.0 °F
DAM; ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 263 °C
505 °F
DAM; 10°C/min; ISO 11357-1/-3
Descriptive Properties Value Comments
Additives Release agent
Delivery Form Pellets
Part Marking Code >PA-IGF40<
ISO 11469
Processing Injection Moulding
Regional Availability Asia Pacific
Europe
Global
Near East/Africa
North America
South and Central America
Resin Identification PA-IGF40
Special Characteristics Heat stabilised or stable to heat
Users viewing this material also viewed the following: