Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 2.14 GPa @Strain 3.20 %, Temperature 0.000 °C |
311 ksi @Strain 3.20 %, Temperature 32.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 900P NC010 Acetal (POM)
(Unverified Data**) Low Viscosity Acetal Homopolymer with Improved Processing Delrin 900P is a low viscosity acetal homopolymer for injection molding. It has improved processing thermal stability good mechanical proper.. |
|||
Secant Modulus | 2.14 GPa @Strain 3.20 %, Temperature 0.000 °C |
311 ksi @Strain 3.20 %, Temperature 32.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® FG900P NC010 Acetal (POM)
(Unverified Data**) Low Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG900P is a low viscosity acetal homopolymer with improved thermal stability. It has been developed for consideration .. |
|||
Secant Modulus | 2.14 GPa @Strain 1.40 %, Temperature 80.0 °C |
310 ksi @Strain 1.40 %, Temperature 176 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Minlon® 10B40 NC010 Nylon 66
(Unverified Data**) 40% Mineral Reinforced Polyamide 66Minlon 10B40 NC010 is a 40% mineral reinforced polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |