Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 2.61 GPa @Strain 2.70 %, Temperature -40.0 °C |
378 ksi @Strain 2.70 %, Temperature -40.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® S600F40 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l Unreinforced Low Viscosity Polybutylene Terephthalate Crastin S600F40 NC010 is an unreinforced lubricated low viscosity polybutylene terephthalate resin for injection molding.Information provided by.. |
|||
Secant Modulus | 2.61 GPa @Strain 1.10 %, Temperature 100 °C |
378 ksi @Strain 1.10 %, Temperature 212 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Minlon® IG38C1 BK434 Nylon 66