Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Secant Modulus = 2.71 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus 2.71 GPa

@Strain 1.30 %,
Temperature 200 °C
393 ksi

@Strain 1.30 %,
Temperature 392 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® HTN 51G35EF BK083 Polyphthalamide (PPA)  (Unverified Data**)
35% Glass Reinforced PPA High Performance Polyamide Developed for Electrical and Electronics Applications Zytel HTN51G35EF BK083 is a 35% glass reinforced heat stabilized lubricated high performance..
Secant Modulus 2.71 GPa

@Strain 1.30 %,
Temperature 200 °C
393 ksi

@Strain 1.30 %,
Temperature 392 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® HTN 51G35HSL BK083 Polyphthalamide (PPA)  (Unverified Data**)
35% Glass Reinforced PPA High Performance Polyamide Zytel HTN51G35HSL BK083 is a 35% glass reinforced heat stabilized lubricated high performance polyamide resin. It is also a PPA resin.Information ..
Secant Modulus 2.71 GPa

@Strain 2.50 %,
Temperature 23.0 °C
393 ksi

@Strain 2.50 %,
Temperature 73.4 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Minlon® IG38C1 BK434 Nylon 66  (Unverified Data**)
38% Mineral/Glass Reinforced Polyamide 66 Minlon IG38C1 BK434 is a 38% mineral/glass reinforced heat stabilized black polyamide 66 resin for injection molding.Information provided by DuPont Performa..
Secant Modulus 2.71 GPa

@Strain 1.30 %,
Temperature 80.0 °C
393 ksi

@Strain 1.30 %,
Temperature 176 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Minlon® IG38C1 BK434 Nylon 66  (Unverified Data**)
38% Mineral/Glass Reinforced Polyamide 66 Minlon IG38C1 BK434 is a 38% mineral/glass reinforced heat stabilized black polyamide 66 resin for injection molding.Information provided by DuPont Performa..
Secant Modulus 2.71 GPa

@Strain 2.64148 %,
Temperature 80.0 °C
393 ksi

@Strain 2.64148 %,
Temperature 176 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® SK615SF NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)&l
30% Glass Reinforced Low Viscosity Polybutylene Terephthalate Developed for Super Fast Production Crastin SK615SF is a 30% glass fiber reinforced low viscosity polybutylene terephthalate for injecti..
Copyright © lookpolymers.com All Rights Reserved