Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 1.76 GPa @Strain 6.00 %, Temperature -40.0 °C |
255 ksi @Strain 6.00 %, Temperature -40.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 311DP BK402 Acetal (POM)
(Unverified Data**) Nucleated Medium-high Viscosity Acetal Homopolymer Delrin 311DP BK402 is a medium high viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding(reduced.. |
|||
Secant Modulus | 1.76 GPa @Strain 3.50 %, Temperature 23.0 °C |
255 ksi @Strain 3.50 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 900P NC010 Acetal (POM)
(Unverified Data**) Low Viscosity Acetal Homopolymer with Improved Processing Delrin 900P is a low viscosity acetal homopolymer for injection molding. It has improved processing thermal stability good mechanical proper.. |
|||
Secant Modulus | 1.76 GPa @Strain 3.50 %, Temperature 23.0 °C |
255 ksi @Strain 3.50 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® FG900P NC010 Acetal (POM)
(Unverified Data**) Low Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG900P is a low viscosity acetal homopolymer with improved thermal stability. It has been developed for consideration .. |
|||
Secant Modulus | 1.76 GPa @Strain 1.50 %, Temperature 80.0 °C |
255 ksi @Strain 1.50 %, Temperature 176 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK641FR NC010 Polybutylene Terephthalate (PBT) 10% Glass Reinforced Flame Retardant Polybutylene Terephthalate Information provided by DuPont Performance Polymers |
|||
Secant Modulus | 1.76 GPa @Strain 3.39 %, Temperature 23.0 °C |
255 ksi @Strain 3.39 %, Temperature 73.4 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 151L NC010 Nylon 612
(Unverified Data**) Unreinforced Polyamide 612Information provided by DuPont Performance Polymers |