Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 3.78 GPa @Strain 1.40 %, Temperature 100 °C |
549 ksi @Strain 1.40 %, Temperature 212 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® PLS 95G40DH1T BK261 Nylon 6
(Unverified Data**) 40% Glass Reinforced Heat Stabilized Polyamide Zytel PLS95G40DH1T is a 40% GR impact modified PA made with SHIELD technology its superior heatInformation provided by DuPont Performance Polymers |
|||
Secant Modulus | 3.78 GPa @Strain 2.30 %, Temperature 100 °C |
548 ksi @Strain 2.30 %, Temperature 212 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN 51G45HSL NC010 Polyphthalamide (PPA)
(Unverified Data**) 45% Glass Reinforced PPA High Performance Polyamide Zytel HTN51G45HSL NC010 is a 45% glass reinforced heat stabilized lubricated high performance polyamide resin. It is also a PPA resin.Information .. |