Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 4.47 GPa @Strain 2.08 %, Temperature 40.0 °C |
649 ksi @Strain 2.08 %, Temperature 104 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Rynite® FR515 NC010 Polyethylene Terephthalate (PET)
(Unverified Data**) 15% Glass Reinforced Flame Retardant Polyethylene Terephthalate Rynite FR515 NC010 is a flame retardant 15% glass reinforced modified polyethylene terephthalate. Recognized by UL as UL94V-0 at 0.8mm.. |