Polymer Property : Secant Modulus = 406 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus 2.80 GPa

@Strain 2.90 %,
Temperature 100 °C
406 ksi

@Strain 2.90 %,
Temperature 212 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 70G33HS1L NC010 Nylon 66  (Unverified Data**)
33% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G33HS1L NC010 is a 33% glass fiber reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Perfor..